Anyone who needs a thread or a bracket on sheet metal has several options. Here we compare stud welding with riveting, screwing and press-in fasteners and show when each method makes sense.
In short
Stud welding needs no drilled hole and access from only one side. Compared with rivets, screws and press-in fasteners, this saves work steps and does not weaken the component. Those methods remain useful when the materials are not weldable or no heat may be introduced.
On this page
Stud welding or riveting: which is better?
Stud welding is usually faster and cleaner, because no hole has to be drilled. A blind rivet or rivet nut always needs a hole, which weakens the component and its surface and allows moisture to penetrate. The weld stud, on the other hand, is placed on the closed sheet in milliseconds. Rivets remain useful when the materials are not weldable or no heat at all may be introduced.
What are the advantages over screws?
A screw connection needs a drilled hole and often a nut on the back, so access from both sides is required. The weld stud needs only one side, and drilling, tapping and deburring are no longer necessary. This saves work steps, and with tip ignition the back can even remain invisible, depending on the application.
Stud welding or press-in nuts?
Press-in fasteners also need a pre-punched or drilled hole, a minimum sheet thickness and a press. Stud welding works without a hole and also on very thin sheet. Press-in fasteners, on the other hand, have the advantage when punched holes already exist or welding is not permitted.
What are the advantages of stud welding at a glance?
- access from only one side required
- no drilled hole, so sealed sheets and no weakening of the component
- very short welding time from milliseconds up to about one second
- full fusion over the entire stud end face
- with tip ignition, no marks on the visible side depending on the application
- easy to automate, from the automatic welding gun to the CNC system
Where does stud welding reach its limits?
The base material and the stud must be weldable, and for most processes the surface must be clean. A welded stud cannot be unscrewed again, only the nut on it. In addition, an investment in a welding unit and gun is necessary. For individual projects, however, you can also rent units from Arnhold.
Would you like to know whether stud welding is the better solution for your component?
We will be happy to advise you personally, by phone on +49 2302 95640-0 or by message.