Drawn Arc (ARC)

Large studs and high-quality welds: this is what makes the drawn arc (ARC) processes so convincing. Here you will find the scope of application, the three variants of the process and the technical data.

In short

In drawn arc welding, the stud is lifted from the workpiece under a pilot arc and plunges into the molten pool after the welding time. The process is suitable for studs from 2 to 25 mm and many stud shapes, from threaded studs to concrete anchors. There are three variants: the short-cycle process, drawn arc welding with ceramic ferrule and drawn arc welding with shielding gas.

Steel tube with welded hook studs, drawn arc welding

Which studs is drawn arc welding suitable for?

Drawn arc welding is suitable for studs from 2 mm to 25 mm, and a wide variety of stud shapes can be welded. Above all, threaded studs, pins, insulation pins, bayonet pins, internally threaded bushes, concrete anchors and flat anchors made of St37, 15Mo3, 1.4301, 1.4713/42/62 and 1.4841 are possible.

What variants of drawn arc welding are there?

Drawn arc welding is divided into three main processes: stud welding with the short-cycle process, with ceramic ferrule and with shielding gas. On the following pages, all three are explained in more detail, with application strengths and technical details.

Short-cycle

Very short welding time, ideal for thinner sheet, curved surfaces and automation.

Ceramic ferrule

The ceramic ferrule protects the molten pool and forms the weld collar. For large studs and longer welding times.

Shielding gas

The shielding gas protects the molten pool from the air. For very high-quality, visually appealing welds.

What technical data apply?

ParameterShort-cycleCeramic ferruleShielding gas
Stud size d (mm) 2-10 5-25 2-12
Peak current approx. (A) 300-1900 300-3000 300-3000
Welding time approx. (ms) 5-100 100-2000 5-2000
Surface Bare metal, galvanised
(suitable for poorer surfaces)
Bare metal, flash rust, mill scale
(rougher surfaces)
Bare metal, galvanised
(suitable for poorer surfaces)
Min. workpiece thickness (mm) 1/8 d (stud) 1/4 d (stud) 1/8 d (stud)
Ceramic ferrule required no yes no
Shielding gas function required partly no yes
Visual appearance of the weld good good very good
Lower-cost studs yes no no
Insulation applications yes yes yes
Material St, VA, MS, AL
(and others)
St37, 15Mo3, 1.4301, 1.4713/42/62, 1.4841
heat-resistant
St37, 15Mo3, 1.4301, 1.4713/42/62, 1.4841
heat-resistant
Application strengths
  • Very high process reliability
  • Works well on poor surfaces
  • Easy to automate
  • Drawn arc welding on thin sheet
  • Required for drawn arc studs with d > 5 mm and longer welding times to stabilise the weld pool
  • Ceramic ferrule has a positive effect on the weld structure
  • Use with large studs
  • Produces considerably higher-quality welds
  • Avoids porosity
  • Focuses the energy at the weld spot
  • Easy to automate (pick-up method for large studs)
Good to know
  • Deeper penetration than tip ignition, so marks and temper colours on the back are more likely
  • Higher weld collar may make assembly more difficult in some cases
  • Can be automated to a limited extent
  • Requires ceramic ferrules
  • Ceramic ferrules must be fitted individually
  • Ceramic ferrules cannot be fed automatically
  • Very deep penetration
  • Requires a shielding gas function on the unit
  • Produces very high-quality, visually appealing welds
  • More sensitive to arc blow at workpiece edges and with asymmetrical earth points
Values may vary depending on unit and application

Would you like to know which drawn arc variant suits your component?

We will be happy to advise you personally, by phone on +49 2302 95640-0 or by message.

Send an enquiry

More topics

Processes

Tip ignition or drawn arc? All processes at a glance.

Tip ignition

Strengths, applications and key data at a glance.

Materials

Stainless steel, aluminium, galvanised sheet and more.

Arc blow

Causes of one-sided weld collars and how to avoid them.