In a properly executed stud weld, the weld is not the weak point. Here you can find out what the load capacity depends on, how to test the quality and which standards apply.
In short
In a properly executed weld, the joint does not fail in the weld zone but in the stud or the base material. Quality is usually checked with a visual inspection and a bend test. The most important standards are DIN EN ISO 14555 for the process and DIN EN ISO 13918 for the studs.
On this page
How strong is a stud weld?
In a properly executed weld, the joint does not fail in the weld zone but in the stud or in the base material. The load capacity is therefore determined by the stud material, its stress cross-section and the base material. A steel stud of property class 4.8, for example, has a yield strength of at least 340 N/mm², and stainless steel A2-50 has a tensile strength of at least 500 N/mm².
What does the strength depend on?
The most important factors are the stud material and diameter, the material and thickness of the sheet, and the quality of the weld itself. Deviations are possible with studs that have a reduced weld area, such as mini flange studs, and with mixed joints of steel and stainless steel. If in doubt, the quality is verified by a welding procedure test.
What torque can I use to tighten the nut?
The permissible tightening torque depends on the thread size, the stud material and the wall thickness of the component. Recommended assembly torques can be found in the technical information on our tip ignition studs. The values apply to standard threads without lubrication and must be adapted to the specific application.
How do you test a stud weld?
The simplest way is a visual inspection and a bend test: the stud is bent, and the weld must not crack. For threaded studs, a torque test is also common. In series production, systems with weld data monitoring automatically rate every weld as OK or not OK.
Which standards apply to stud welding?
The most important standards are DIN EN ISO 14555 for arc stud welding and DIN EN ISO 13918 for studs and ceramic ferrules. In addition, there are the DVS guidelines, for example DVS 0903 on tip ignition. For the calibration of welding equipment, DIN EN ISO 17662 and the DVS guidelines 0714 and 3009 apply.
What are typical defects in stud welding?
The most common causes of poor welds are:
- wrong parameters for the stud, material or sheet thickness
- dirty, painted or oily surfaces
- poor or one-sided earth connection, which leads to arc blow
- welding gun not placed perpendicular to the surface
- studs from different production batches mixed together
You can find more about one-sided weld collars on our page about arc blow.
What do I need to consider for safety?
Stud welding produces a bright arc, spatter, a loud bang and welding fumes. Wear eye protection, hearing protection and suitable work clothing, and make sure there is fume extraction when welding galvanised sheet. Employees who are new to stud welding should receive instruction or training beforehand.
Would you like to ensure the quality of your stud welds?
We will be happy to advise you personally, by phone on +49 2302 95640-0 or by message.
More topics
What is stud welding and how does it work?
Tip ignition or drawn arc? All processes at a glance.