Wullener Feld 48, 58454 Witten +49 2302 956400 This email address is being protected from spambots. You need JavaScript enabled to view it.

Select your language

Banner2000x200

Tip Ignition (CD)

Easy handling and high quality on thin sheet: this is what makes the tip ignition (CD) processes so convincing. Here you will find the strengths, typical applications and variants of the process as well as the technical data.

In short

In tip ignition, the arc forms via the ignition tip of the stud with a very high current and within a few milliseconds. The process is suitable for studs from 0.8 to 8 mm on sheet from 0.5 mm, and the units run on a standard 230 V socket. There are two variants: the contact method and the gap method.

Front panel with welded tip ignition studs

What are the advantages of tip ignition?

  • low-cost weld studs
  • a standard 230 V AC socket is sufficient
  • easy handling
  • low-cost units
  • easy to automate
  • no marks or, depending on the application, only faint marks on the reverse side
  • painted reverse sides possible

Where is tip ignition used?

Typical applications are control cabinet construction, vehicle construction, façade technology, cathodic corrosion protection and insulation on metal.

What variants of tip ignition are there?

The tip ignition process is divided into the contact method and the gap method. On the following pages, both methods are explained in more detail, with application strengths and technical details.

Contact method

The stud rests on the sheet with its ignition tip before welding. Strong for manual welding of steel and on galvanised and slightly curved surfaces.

Gap method

The stud is held at a small distance and only placed on the sheet during welding. Strong on aluminium, on thin sheet with high requirements for the back and in automated welding.

Where are the process limits?

The basic rule also applies to stud welding: the joint must not fail in the fusion zone. During the extremely short welding time, the entire surface of the weld stud and the workpiece must be melted. This results in process limits beyond which compromises in strength must be accepted.

The following table shows dimensions with which process-reliable joints according to DVS can be achieved. Other dimensions can in some cases be welded well and reliably, but should be checked by tests on the actual welding task. A welding procedure test according to DIN EN ISO 14555 can usually only be passed with considerable effort.

What technical data apply?

ParameterGap weldingContact welding
Process no. according to ISO 4063 786 786
Stud diameter d (mm) 0.8 to 8 (aluminium up to 6) 0.8 to 8 (aluminium up to 6)
Peak current approx. (A) 10,000 10,000
Welding time approx. (ms) 0.5-2 1-4
Spring force approx. (N) 40-60 60-100 (depending on piston dimensions and bearing)
Impact speed approx. (m/s) 0.5-1 (aluminium 1-1.5) 0.5-0.7
Ignition Mostly correct (early ignition possible),
high process reliability
Always correct,
high process reliability
Barely visible marks on the back yes yes
Material St, VA, MS, AL
(and others)
St, VA, MS, AL
(and others)
Min. workpiece thickness (mm) 0.5 0.5
Insulation applications yes yes
Application strengths
  • Automated welding
  • Thin sheet with high requirements for the back
  • Aluminium
  • Manual welding of steel (alloyed/unalloyed)
  • Galvanised surfaces
  • Slightly curved surfaces
Use outside the process limits
Geometric limit
  • < Ø10, Ø12 in steel, stainless steel and brass
  • < Ø8 in aluminium
(These joints are possible, but fracture in the weld zone cannot always be ruled out.)
Limit of weldability of the workpiece material
  • unsuitable coatings, some exceeding 25 µm (e.g. galvanising)
  • thick coatings combined with large diameters
  • oxides on aluminium surfaces
  • alloying elements such as lead, sulphur
Values may vary depending on unit and application

The values in the table above are based on Table 1 of DVS 0903:2018.

Would you like to know whether tip ignition suits your component?

We will be happy to advise you personally, by phone on +49 2302 95640-0 or by message.

Send an enquiry

More topics

Processes

Tip ignition or drawn arc? All processes at a glance.

Drawn arc

Scope, variants and key data at a glance.

Materials

Stainless steel, aluminium, galvanised sheet and more.

Strength

Load capacity, testing and standards.